- Home
- 3D Printing
- How to 3D Print TPU: Flexible Filament Guide
How to 3D Print TPU: Flexible Filament Guide
Sooner or later you want to print something that bends: a bumper for a gadget, a foot that stops a speaker buzzing on a shelf, a gasket that actually seals. That’s the moment people discover TPU, the flexible filament that behaves more like rubber than plastic. They also discover that their first print looks like a bird’s nest. The good news is that how to 3D print TPU is mostly one idea repeated: give the filament no room to misbehave, then go slowly.
Why TPU is different from everything else on the spool rack
PLA and PETG are stiff. You can push them through an extruder like a thin rod, and that rod goes exactly where the gears send it. TPU is a thermoplastic polyurethane, and it squashes and stretches. Push too hard from behind and it doesn’t advance, it buckles sideways into any gap it finds. Pull too hard on retraction and it stretches instead of backing out. Almost every TPU failure traces back to one of those two behaviours.
That also explains why the printer matters more here than with any other material. On a direct-drive extruder, the gears sit a few centimetres above the nozzle, so there’s little unsupported filament between the push and the melt. On a Bowden setup, the drive gear lives at the frame and a long PTFE tube carries the filament to the hotend. Firm TPU can still make that trip, because the tube supports it, but soft grades compress and spring like a squeezed sponge, and you get under-extrusion that no slicer setting fully cures.
If you’re deciding on a machine partly for this kind of work, our best 3D printers guide flags which models ship with direct drive, and the closed-chamber machines in our Bambu Lab review have profiles for flexible spools that take much of the guessing away. Budget machines such as those in our Creality review can print TPU too, usually with a little more tuning and a printed or bought filament guide.
Hardness: picking the right grade
TPU is sold by Shore hardness, written as a number followed by “A”. The lower the number, the softer the part and the harder the print. As a rough map from what makers and the printing community commonly report:
| Grade | Feels like | Difficulty | Good for |
|---|---|---|---|
| 85A | Soft rubber band | Hard, wants direct drive and patience | Seals, soft grips, very bendy parts |
| 90A | Flexible shoe sole | Moderate | Wearables, soft feet, gaskets |
| 95A | Firm silicone, bike grip | Easiest common grade | Phone cases, bumpers, wheels, mounts |
| 98A and up | Tough, slightly bendy plastic | Easy | Parts needing some give but real strength |
If this is your first spool, buy 95A. It still stretches and absorbs a knock, but it’s firm enough that a typical extruder can push it without drama. You can always move softer once you trust your setup. A very soft first spool is the single most common reason people decide “my printer can’t do TPU” when the real culprit was the choice of grade.
Dry it before you do anything else
TPU drinks moisture, and the symptoms are easy to mistake for a settings problem: tiny bubbles popping at the nozzle, hairy strings between features, a dull and rough surface, weak layers. Before you touch a slicer slider, dry the spool. We’d say this is the cheapest fix in all of 3D printing, and our piece on whether you need a filament dryer goes through the options. For flexible filament it’s closer to mandatory than optional. Follow the temperature printed on the spool, since TPU softens at lower temperatures than people assume, and keep the spool sealed with desiccant when you’re not printing.
The settings that matter
Every brand publishes its own recommended window on the label or product page, and that always beats a number from an article, ours included. What follows are sensible starting points that many people report working on direct-drive machines, not laws.
Nozzle temperature usually lands somewhere between 220 and 240 °C, with the bed at 50–60 °C. Speed is where TPU asks for humility: begin around 20–30 mm/s, and make the first layer slower still. It will feel absurdly slow compared with PLA, but the extruder can only push so fast before the filament starts compressing, and a steady slow print beats a fast failed one. Some modern high-flow setups handle certain spools at higher speeds, which is fine, but treat that as an upgrade after the first success.
Retraction is the setting people get wrong most. With PLA, a bit of retraction fights stringing. With TPU, long fast retraction stretches the filament and can lead to jams. Start with retraction off or a very short distance at low speed, and add it back only if the strings bother you. Part cooling can usually stay moderate; TPU doesn’t need the roaring fan PLA enjoys, and too much cooling hurts layer adhesion.
These bars are our editorial read of how forgiving each combination tends to be for a hobbyist, drawn from what makers and users commonly report, not from measurements of our own.
Bed, first layer and removing the part
TPU sticks readily, which is helpful until it isn’t. A textured PEI sheet is the friendliest option; it grips the first layer and releases once cooled. On smooth PEI, TPU can bond so well that prying risks tearing the surface, so a thin film of glue stick works as a release layer. Let the bed cool fully, then flex the plate rather than levering at the part. If you fight adhesion problems early on, our guide to fixing bed adhesion applies here too, with the caveat that TPU usually needs a gentler first-layer squish than PLA.
Keep the filament path tight. Many people print or buy a small guide that supports the filament right at the extruder entrance, closing the gap where soft filament likes to fold. Loosen the extruder tension a bit, because crushing the filament between the gears causes its own jams, and make sure the spool unwinds freely so the extruder isn’t dragging against resistance.
Troubleshooting without guessing
When a TPU print goes wrong, resist the urge to change five things. Change one, print a small test, then move on.
If you see grinding or the filament folding at the extruder, you’re pushing too fast or the path has a gap: slow down and check the guide. Under-extrusion with clicking usually means a partial clog or too much speed, and a slightly warmer nozzle can help. Stringing and wispy hair point first at moisture, then at temperature, which is why stringing fixes start with the spool rather than the slicer. Blobs and zits on corners are usually retraction fighting the elasticity, so shorten it. If supports fuse to the part, accept that TPU supports are miserable and design around them where you can, with chamfers instead of overhangs and bridges kept short.
Wall count and infill change how a part feels. Few walls and low infill give a squishy, compressible object. More perimeters and a denser infill pattern stiffen it dramatically, which is how you tune a single filament from soft grip to firm bumper without changing spools.
What TPU is actually good for
Think about parts that take a hit or seal a gap. Phone and controller cases, shock-absorbing feet for speakers and printers, vibration pads under a small motor, gaskets and o-rings for low-pressure jobs, drone landing gear and camera dampers, little wheels and tyres for a hobby robot, wearable straps. If you’re building around a quadcopter or a small robot, TPU parts are a fast way to protect expensive electronics, and they pair nicely with the repair-minded ideas in our guide to printing replacement parts for the home.
TPU is a bad idea for anything that must stay accurate and stiff, like a tight-tolerance bracket or a precise gear, and it doesn’t love continuous heat. For tough, slightly flexible parts that print more easily, PETG often does the job with half the fuss.
What we'd tell a friend
- Buy 95A first; go softer only once your setup is proven.
- Dry the spool, then print slowly, around 20–30 mm/s to start.
- Keep retraction short or off, and close any gap around the filament.
- Change one setting at a time and print a small test, not the final part.
Buying a first spool
For a first try, a 1.75 mm spool of 95A TPU in a neutral colour from an established maker is the safe pick, since transparent and unusual colours can behave differently. You can browse TPU filament on Amazon and read the reviews for comments on feeding and stringing; users tend to be frank about both. We haven’t put every brand through its paces, so treat any one review as a data point and look for consistent feedback across several. A small spare filament guide is also cheap, and you can find TPU-friendly extruder upgrades if your printer is a Bowden model and flexible filament is a long-term plan. If you’re still learning the basics, our beginner’s guide to 3D printing is a better first stop, and the full 3D Printing category has the rest.